| Mechanische Eigenschaften | |||||||||||||||||||
| Qualitätsstufe | Tempel | Zugfestigkeit Rm/MPa | Dehnung % | Härte | |||||||||||||||
| GB | JIS | ASTM | EN | GB | JIS | ASTM | EN | GB | JIS | ASTM | EN | GB | JIS | ASTM | EN | GB (HV) | JIS (HV) | ASTM (HR) Oberflächlich 30T | EN (HV) | 
| H63 | C2720 | C27200 | CuZn37 | O60 | O | M20 | R300 | ≥290 | ≥275 | 285-350 | 300-370 | ≥35 | ≥40 | - | ≥ 38 | ≤95 | - | - | 55-95 | 
| - | 1/4H | H01 | - | - | 325-410 | 340-405 | - | - | ≥35 | - | - | - | 75-125 | 43-57 | - | ||||
| H02 | 1/2 Stunde | H02 | R350 | 350-470 | 355-440 | 385-455 | 350-440 | ≥20 | ≥ 28 | - | ≥19 | 90-130 | 85-145 | 54-67 | 95-125 | ||||
| - | - | H03 | R410 | - | - | 435-505 | 410-490 | - | - | - | ≥8 | - | - | 64-70 | 120-155 | ||||
| H04 | H | H04 | R480 | 410-630 | ≥410 | 485-550 | 480-560 | ≥10 | - | - | ≥3 | 125-165 | ≥105 | 67-72 | 150 bis 180 | ||||
| H06 | - | H06 | R550 | ≥585 | - | 560-625 | ≥ 550 | ≥2,5 | - | - | - | ≥155 | - | 71-75 | ≥170 | ||||
| Qualitätsstufe | Hauptbestandteile % | Dichte (g/cm³) | Modul der Elastizität (GPa) | Koeffizient der thermischen Ausdehnung (×10 -6/K) | Elektrische Leitfähigkeit (%IACS) | Wärmeleitfähigkeit (W/(m·K)) | ||||||
| Cu | Cu+Zn | |||||||||||
| H63 | 62,0-65,0 | ≥99,7 | 8.43 | 105 | 20.2 | 23 | 120 | |||||